Jul 10, 2025 Tinggalkan pesanan

ASTM A335 Alloy Steel Pipe: Grades, Composition and Mechanical Properties

What Is ASTM A335 Pipe?

ASTM A335 is the standard specification for seamless ferritic alloy steel pipe for high-temperature service. The grades covered are chromium-molybdenum steels, and some of the newer grades also contain vanadium, niobium and nitrogen. The specification defines chemistry, heat treatment, tensile and yield requirements, elongation, hardness limits, dimensional tolerances and testing for pipe intended to operate in the creep range - steam lines, boiler outlet piping, refinery process lines and similar duties.

All product under this specification is seamless. That is the essential difference between A335 pipe and welded alternatives, and it is why A335 is specified for the hottest and highest-pressure lines where a longitudinal seam would be unacceptable.

Grades are written with a P prefix followed by a number that expresses the nominal chromium content. The table below shows the alloying pattern for the most widely used grades; carbon, manganese, silicon and residual limits are fixed by the specification for each grade.

P5 5Cr-Mo 4.00-6.00 0.45-0.65
P9 9Cr-Mo 8.00-10.00 0.90-1.10
P11 1-1/4Cr-Mo 1.00-1.50 0.44-0.65 General elevated-temperature grade
P22 2-1/4Cr-Mo 1.90-2.60 0.87-1.13 Higher temperature capability than P11
P91 9Cr-1Mo-V 8.00-9.50 0.85-1.05

The pattern is progressive: as chromium and molybdenum rise, oxidation resistance and creep strength rise with them, and so does the fabrication discipline required. The vanadium and niobium additions in the 9Cr-1Mo-V grade are what give it its much higher elevated-temperature strength compared with the simple Cr-Mo grades.

Room-temperature tensile strength across the grade range generally falls between about 415 and 620 MPa, with yield strength between about 205 and 415 MPa, depending on the grade and the heat-treatment condition supplied. Elongation is normally 20% or better, which ensures the toughness needed for bending and field welding. Higher-chromium grades sit at the top of the strength band - the 9Cr-1Mo-V grade, for example, has a minimum tensile strength of 585 MPa and a minimum yield strength of 415 MPa. Hardness is controlled within limits that balance machinability against wear and creep performance, and is verified in accordance with the applicable test method.

A335 pipe is designed for high-temperature service, and the useful range of each grade is determined by its allowable stress at temperature:

Lower-alloy grades such as P11 are used for moderate elevated-temperature steam and process duty.

P22 extends the range and is common in power station boiler and main steam piping.

P5 and P9 are selected where scaling resistance at higher temperature matters.

P91 and the higher 9Cr grades are used for main steam and hot reheat lines where metal temperatures run well above the capability of simple Cr-Mo steels.

At the low end, toughness must be considered for cold service and is verified by Charpy impact testing. At the high end, exceeding the grade's limit accelerates creep deformation and oxidation, so the design temperature must always be checked against the allowable stress table of the construction code for the exact grade and product form.

A335 Compared with A213

A335 A213
Seamless pipe for high-temperature and high-pressure pipelines
Non-destructive examination and pressure testing to the piping specification

A335 pipe is supplied across a wide outside diameter range, from small tube sizes up to heavy-wall pipe for main steam service, with wall thickness selected from the standard schedules or specified as a minimum wall. Lengths of 6 to 12 metres are normal, and cut lengths can be produced to order. Specification should be based on design pressure, design temperature and the corrosivity of the fluid.

Fabrication of Cr-Mo pipe requires preheating before welding, matching low-hydrogen filler metal, controlled interpass temperature and post-weld heat treatment on completion. Heat treatment is not optional on these grades: it tempers the weld heat-affected zone, restores toughness and relieves residual stress. Field welds should be supported by a qualified welding procedure and by hardness checks where the construction code requires them.

Q: What are the main components of A335 steel pipe?
Chromium and molybdenum are the alloying elements that define the grades, with carbon, manganese and silicon present in controlled amounts. The 9Cr-1Mo-V grade also contains vanadium, niobium and nitrogen.

Q: What are the mechanical properties of A335 pipe?
Tensile strength generally falls between about 415 and 620 MPa and yield strength between about 205 and 415 MPa depending on grade and heat treatment, with elongation typically 20% or better.

Q: What temperature range is A335 pipe suitable for?
It is designed for high-temperature service, with the specific limit set by grade. Low-alloy grades serve moderate elevated-temperature duty while 9Cr grades serve the hottest main steam and hot reheat lines.

Q: What is the difference between A335 and A213?
A335 covers seamless pipe for high-temperature and high-pressure pipelines with an emphasis on creep and pressure resistance, while A213 covers seamless tube for boilers and heat exchangers with an emphasis on heat transfer and surface quality.

Q: What are the common specifications of A335 pipe?
Outside diameters range from small tube sizes up to large-diameter heavy-wall pipe, with wall thickness taken from standard schedules or specified as a minimum wall, and lengths commonly 6 to 12 metres.

Q: Does A335 pipe need post-weld heat treatment?
Yes, in normal practice. Chromium-molybdenum welds are preheated, welded with matching low-hydrogen filler and then heat treated to temper the heat-affected zone and relieve residual stress.