Apr 02, 2024 Tinggalkan pesanan

Cerucuk Paip ASTM A252 Gred 3

Penerangan Produk

GNEE membekalkan cerucuk paip keluli dalam standard ASTM A252 seperti syarat di bawah:
Gred: 1, 2, dan 3
Dimensi: Sehingga 48 inci lancar dan dikimpal

Jenis: Lancar, Dikimpal (ERW, LSAW, SSAW, DSAW)
Ketebalan: Jadual STD, 40, XS, 80, XXS, 160
Panjang: 6m, 12m atau disesuaikan.
Berakhir: Beveled, Plain
Rawatan Salutan: FBE, 3PE, Bergalvani

Sifat mekanikal standard ASTM a252

Gred

Darjah 1

Darjah 2

Darjah 3

Kekuatan Tegangan, Min psi

50,000

60,000

66,000

Kekuatan Hasil, Min psi

30,000

35,000

45,000

Carta Saiz Cerucuk Paip Gred 3 A252

dinding Saiz ( OD)
.010 1/16" , 1/8" , 3/16"
.020 1/16" , 1/8" , 3/16" , 1/4" , 5/16" , 3/8"
.012 1/8"
.016 1/8" , 3/16"
.028 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 3/4" , 1" , 1 1/2" , 2"
.035 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 7/16" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.049 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/8" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.065 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 3/4" , 2" , 2 1/2" , 3"
.083 1/4" , 3/8" , 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 7/8" , 2" , 2 1/2" ,3"
.095 1/2" , 5/8" , 1" , 1 1/4" , 1 1/2" , 2"
.109 1/2" , 3/4" , 1" , 1 1/4" , 1 1/2" , 2"
.120 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 2" , 2 1/4" , 2 1/2" , 3"
.125 3/4" , 1" , 1 1/4" , 1 1/2" , 2" , 3" , 3 1/4"
.134 1"
.250 3"
.375 3 1/2"

Cerucuk paip keluli A252